Components for Electron Tubes

Cup grids made of molybdenum Electron tubes for power technology and telecommunications contain a vacuum and their cathode has to be heated to very high temperatures in order to emit a constant stream of electrons.

PLANSEE products and components are tailor-made for tube parts with high thermal load.

Advantages:

  • Extreme high-temperature resistance
  • Low vapour pressure at high temperatures
  • Strength at high temperatures 

Forms of delivery:

Finished parts:

  • Seamless cups made of Mo and W
  • Mo rings
  • Mo tubes

Semi-finished products:

  • Sheets, foils, rods made of Mo and W