Evaporation Boats

Evaporation boats Materials used for evaporation sources such as boats, coils or crucibles must show a good electrical conductivity, a high melting point and a low evaporation pressure. PLANSEE offers evaporation boats made of various materials which cover a wide range of applications.

Materials:

  • Tungsten
  • Molybdenum
  • Molybdenum 0,3% Lanthan (ML): do have multiple life-time for many applications than pure Mo
  • Molybdenum Yttriumoxide (MY): do have multiple life-time for many applications than pure Mo
  • Tantalum 

Advantages:

  • Long life-time owing to high and constant product quality
  • Dimensional accuracy: easy to handle

Based on our experience for many years we can also improve the efficiency of  existing evaporation boats for example by modifying the design or the clamping device.

Forms of delivery:

Finished products:

  • All kinds of shaped or folded boats, pickled or bright, in cardboard boxes with labels

Semi-finished products:

  • Ribbons and sheets in standard and deep drawn quality