Sintering Boats, Stacking Sheets and Base Plates
For various sintering and annealing processes, for example in metal injection moulding (MIM), in lamp manufacturing, in the production of fuel elements for nuclear power or in the production of tantalum capacitors, PLANSEE furnace boats and stacking sheets are used to bring the workpiece into the furnace. In pusher furnaces the sintering boats are usually placed on heavy base plates (skids), which take the pushing force.
 |
Because of its improved dimensional stability and lifetime in comparison to pure molybdenum, the PLANSEE high-performance material MLR in particular has become established as a type of standard in many applications of these components. |
Advantages:
- Use of PLANSEE high-performance materials with excellent creep resistance and structural stability
- Low distortion and high dimensional stability
- Many design possibilities
Available Products:
- Boats in Mo, MLR, TZM, Ta or W in riveted, deep-drawn of folded construction