Materials testing includes mechanical testing, non-destructive testing and microstructural analysis of metals and alloys.Characteristic values from tests are stored in the database „Alloys-DB“ according to the material type.

Equipment

Performance

Field of use

Mechanical testing    

Tensile testing

Range of force: 50 N to 1 MN
Temperature range: room-temperature up to 2200 °C
Testing atmospheres: air, vacuum or protective atmospheres

Tensile-, compression-, bending- and sheartesting;
Determination of the Young´s Modulus;
Short term creep tests;
Determination of Poisson´s ratio at room temperature

Fatigue testing

Resonant machine
Range of force: 20 kN
Temperature range: room-temperature up to 1100 °C
Testing atmosphere: air

Determination of fatigue strength of high performance materials
Hardness testing Vickers-, Rockwell-, Brinell-, shorehardness  Determination of hardness of components

Non-destructive testing

Ultrasonic testing

Handheld probe and ultrasonic scanner with water bath;
Testing frequency up to 20 MHz
A-, B- and C-Scan
Detection of voids in components
Radiography X-ray tube
Medium frequency device with a power of
275 kV and 3 mA (focal spot size: 1.5 mm)
Testing of welded and brazed joints
Eddy current testing Handheld probe; Scanner
Multiple frequency method
Coating thickness measurements of laminates
Thermography Infrared camera
Excitation by ultrasound, Lock-In and transient methods
Testing of brazed joints in components
Dye penetration testing visible dye; fluorescent methods Detecting of surface cracks

Metallography & Microspcopy

 

Extensive metallographic equipment Optical microscopes (bright- and dark fi eld, polarised light);
quantitative microstructural analysis
Particle size distribution determination in ODS alloys
Portable metallography Mobile station with grinding and polishing equipment, etching device and microscope

Examination of large parts in the rolling mill

Scanning electron microscope with EDX detector Secondary- and backscatter electron detector; Point-, line- and area analysis Assessment of failure modes in metals