"Molybdenum - Material properties and applications"

TZM (Titanium-Zirconium-Molybdenum)

TZM is a solid-solution hardened and particle-strengthened molybdenum based alloy. The development of a Mo-Ti solid solution and the fine dispersed Ti-carbides are responsible for the excellent strength properties at temperatures up to 1400°C. The average nominal chemical composition in weight%: 0.5 Ti, 0.08 Zr, 0.02 C, remainder Mo.

Advantages compared to pure Mo:

  • better creep resistance
  • higher recrystallization temperature
  • better high-temperature strength
  • better welding properties

Typical areas of application:

  • components for HIP, sintering and heat treatment furnaces
  • metals for rotating anodes for medical diagnostics
  • boats for annealing and sintering processes (temperatures up to 1400 °C)
  • forming tools such as hot runner nozzles for plastic injection moulding
  • moulds for light-alloy casting
  • billets for the isothermal forging