Molybdenum-Copper Composite Materials

Molybdenum/copper from PLANSEE (Elmet, Cunitene or Sparkal) is a powder metallurgical material produced by the means of infiltration with copper contents from 10 to 40 %. Molydenum/copper materials are infiltrated back-cast with copper and can be joined by welding or brazing with various supporting materials. PLANSEE offers MoCu as infiltrated or rolled to sheet material and foils.

 

Advantages of Molybdenum-copper:

  • high arc resistance combined with good electrical conductivity
  • high thermal conductivity
  • low thermal expansion
  • back-castable with copper

 

Typical areas of application:

  • arcing contacts in high and medium voltage breakers for transmission and distribution of electrical power
  • base plates or heat sinks as passive cooling elements of electronic devices
  • erosion electrodes for EDM made of Sparkal
  • electrodes for various applications such as surge protection, welding, brazing and laser applications

 

 Molybdenum: Properties and applications 

 

  Safety data sheet MoCu 

 



How we influence the manufacturing costs and efficiency of CIGS.
[25.01.2012]  
Meet us in Tokyo and Santa Clara!
[13.01.2012]  
Plansee Group sells PMG
[16.12.2011]  
PLANSEE Express offers payment via PayPal
[01.12.2011]  
PLANSEE Tantalum Certified by EICC as „Conflict-Free“
[08.11.2011]  
PLANSEE grows in Korea
[24.10.2011]  
PLANSEE Express online shop opens for American and Canadian markets
[10.10.2011]  
New findings about Laser Structuring of Sputtered Molybdenum
[25.08.2011]  
And the Best Paper Award goes to: PLANSEE.
[18.08.2011]  
Sales increase by 46 percent: Plansee Group achieves best ever figures.
[07.07.2011]  
Blazing heat asks for solid components: PLANSEE at the Thermprocess 2011.
[22.06.2011]  
More efficiency: Molybdenum components for coating facilities.
[09.05.2011]  
Production site in Japan in full operation
[20.04.2011]  
Plansee Group acquires minority ownership of the Chilean company Molibdenos y Metales S.A.
[28.03.2011]  
Online shop now available throughout Europe
[07.02.2011]  
Meet our PVD Coating Team at the SVC in Chicago!
[27.01.2011]  
And the winner is: Multi-leaf collimators for targeted irradiation
[24.01.2011]  
Acquisition of Wolfra-Tech completed
[11.01.2011]  
The right tone - The Plansee wind orchestra released a new CD
[20.12.2010]  
World record with tungsten target
[24.11.2010]  
Revolution at 1,100 kV
[05.11.2010]  
Thorium-free TIG welding electrodes gain in popularity
[28.10.2010]  
On the trail of fine cracks: PLANSEE at the international powder metallurgy conference in Florence
[28.10.2010]  
Thank you for coming. When will we meet again?
[11.10.2010]  
Take the easy way: Sodium doped sputtering targets for CIS/CIGS solar cells.
[27.09.2010]  
Our champion against corrosion at the GLASSTEC. See you in the ring!
[23.09.2010]  
Get to know our strong metals at the ELMIA Subcontractor Show in Sweden
[14.09.2010]  
Sputtering targets for hard coating at the AMB in Stuttgart. Join us!
[08.09.2010]  
PLANSEE Hochleistungswerkstoffe startet Online-Shop
[06.09.2010]  
TiB2 sputtering targets for hard coating at the PSE conference
[06.09.2010]  
Acquisition of Wolfra-Tech: PLANSEE strengthens activities in India
[08.07.2010]  
PLANSEE session at the ESG Conference
[10.06.2010]  
Meet our champion against corrosion
[27.05.2010]  
LED starts with a crucible
[28.04.2010]  
Bi-metal coin: Light as a feather and gleaming blue
[01.04.2010]  
A key component for high-temperature fuel cells
[24.03.2010]  
MoZrO2: Best in corrosion resistance
[23.03.2010]  
Furnace construction expertise for sapphire and silicon melting
[18.02.2010]  
MoZrO2 glass melting electrodes at the Glassman South America
[12.02.2010]  
New sputtering facility supports development of functional coatings
[08.02.2010]  
Multiple-parts solution for arc chambers
[08.02.2010]  
Refractory metals in the glass industry: PLANSEE session in Magdeburg
[03.02.2010]  
Flat screens for China.
[13.01.2010]  
One-stop shop for metallic sputtering targets
[19.11.2009]  
PLANSEE Powertech is preferred strategic supplier of Areva
[16.11.2009]  
Materials and Production Equipment for flat panel display technologies of tomorrow
[09.11.2009]  
Schedule of trade fairs 2009/10
[02.03.2009]  
On the Trail of Future Energy Trends: PLANSEE at international EGT congress
[05.11.2009]  
Direct sales of molybdenum spray wire
[30.10.2009]  
Meet our glass team in Dubai!
[28.10.2009]  
PLANSEE USA celebrates 70 years of business
[22.10.2009]  
Enhanced Glass Tank Performance
[20.10.2009]  
See you in Ohio! PLANSEE at the Glass Problems Conference
[07.10.2009]  
PLANSEE glass team on tour
[02.10.2009]  
Meet us at the PV Conference & Exhibition in Hamburg
[14.09.2009]  
Monolithic rotary sputtering targets
[21.08.2009]  
Plansee Group increases sales in the last fiscal year
[09.07.2009]  
Shaping the future development of growth industries
[25.05.2009]  
17 Plansee Seminar: „Innovation as a basis for future growth”
[25.05.2009]  
Protective sheets for glass-melting tanks
[15.04.2009]  
Sustainable collaboration
[03.04.2009]  
World's largest HIP cyclinder
[20.03.2009]  
Powder Metal community gathers in Reutte
[18.02.2009]  
Covering the entire coatings market
[15.12.2008]  
Plansee Group continues to grow: Sales reach over one billion euros for first time ever
[03.07.2008]  
Plansee Group acquires US powder expert GTP
[23.04.2008]  
The fascination of light: the core for the new 25 Euro coin from PLANSEE
[08.04.2008]  
Schedule of trade fairs 2008/09
[25.03.2008]  
Elektro-Metall becomes PLANSEE Powertech
[12.10.2007]  
Impressing result seen after shut down of a glass tank
[26.11.2007]  
FPD International 2007
[24.10.2007]  
V2007 Vakuumbeschichtung und Plasmaoberflächentechnik
[16.10.2007]  
PLANSEE continues to expand its international presence
[02.03.2007]  
New bimetallic 25-Euro coin - PLANSEE producing the turquoise niobium core
[20.03.2007]  
Plansee Group strengthens its position in North America
[01.12.2006]  
Mathematical simulation for glass tank reinforcements
[21.11.2006]  
PLANSEE with new corporate appearence
[18.09.2006]  
PLANSEE sponsors IIT2006 conference
[29.05.2006]  
FPD & Optoelectronics Show 2006
[19.05.2006]  
Metallurgy Litmash 2006
[10.05.2006]  
"PLANSEE inside"
[24.03.2006]  
SEMICON China 2006
[07.03.2006]  
Change of PLANSEE GmbH to PLANSEE SE
[21.02.2006]  
PLANSEE at SEMICON Korea 2006
[20.01.2006]  
STC certified to aerospace standards AS 9100
[22.12.2005]  
Organizational change at PLANSEE AG
[01.09.2005]  
PLANSEE supplies the violet part of the new bimetallic 25-Euro coin
[22.03.2005]  
Visit us at Glassman Europe 2005
[18.04.2005]  
PLANSEE starts operation of a new hot-forging machine
[06.09.2004]  
25 EURO Coin
[04.05.2004]  
PLANSEE Majority
[04.05.2004]  
 
Archive
Copyright 2012 PLANSEE SE    
All rights reserved.