TZM (Titanium-Zirconium-Molybdenum)

TZM is a solid-solution hardened and particle-strengthened molybdenum based alloy. The development of a Mo-Ti solid solution and the fine dispersed Ti-carbides are responsible for the excellent strength properties at temperatures up to 1400°C. The average nominal chemical composition in weight%: 0.5 Ti, 0.08 Zr, 0.02 C, remainder Mo.

 

Advantages compared to pure Mo:

  • better creep resistance
  • higher recrystallization temperature
  • better high-temperature strength
  • better welding properties

 

Typical areas of application:

  • components for HIP, sintering and heat treatment furnaces
  • metals for rotating anodes for medical diagnostics
  • boats for annealing and sintering processes (temperatures up to 1400 °C)
  • forming tools such as hot runner nozzles for plastic injection moulding
  • moulds for light-alloy casting
  • billets for the isothermal forging



Flat screens for China.
[13.01.2010]  
One-stop shop for metallic sputtering targets
[19.11.2009]  
PLANSEE Powertech is preferred strategic supplier of Areva
[16.11.2009]  
Materials and Production Equipment for flat panel display technologies of tomorrow
[09.11.2009]  
Schedule of trade fairs 2009/10
[02.03.2009]  
On the Trail of Future Energy Trends: PLANSEE at international EGT congress
[05.11.2009]  
Direct sales of molybdenum spray wire
[30.10.2009]  
Meet our glass team in Dubai!
[28.10.2009]  
PLANSEE USA celebrates 70 years of business
[22.10.2009]  
Enhanced Glass Tank Performance
[20.10.2009]  
See you in Ohio! PLANSEE at the Glass Problems Conference
[07.10.2009]  
PLANSEE glass team on tour
[02.10.2009]  
Meet us at the PV Conference & Exhibition in Hamburg
[14.09.2009]  
Monolithic rotary sputtering targets
[21.08.2009]  
Plansee Group increases sales in the last fiscal year
[09.07.2009]  
Shaping the future development of growth industries
[25.05.2009]  
17 Plansee Seminar: „Innovation as a basis for future growth”
[25.05.2009]  
Protective sheets for glass-melting tanks
[15.04.2009]  
Sustainable collaboration
[03.04.2009]  
World's largest HIP cyclinder
[20.03.2009]  
Powder Metal community gathers in Reutte
[18.02.2009]  
Covering the entire coatings market
[15.12.2008]  
Plansee Group continues to grow: Sales reach over one billion euros for first time ever
[03.07.2008]  
Plansee Group acquires US powder expert GTP
[23.04.2008]  
The fascination of light: the core for the new 25 Euro coin from PLANSEE
[08.04.2008]  
Schedule of trade fairs 2008/09
[25.03.2008]  
Elektro-Metall becomes PLANSEE Powertech
[12.10.2007]  
Impressing result seen after shut down of a glass tank
[26.11.2007]  
FPD International 2007
[24.10.2007]  
V2007 Vakuumbeschichtung und Plasmaoberflächentechnik
[16.10.2007]  
PLANSEE continues to expand its international presence
[02.03.2007]  
New bimetallic 25-Euro coin - PLANSEE producing the turquoise niobium core
[20.03.2007]  
Plansee Group strengthens its position in North America
[01.12.2006]  
Mathematical simulation for glass tank reinforcements
[21.11.2006]  
PLANSEE with new corporate appearence
[18.09.2006]  
PLANSEE sponsors IIT2006 conference
[29.05.2006]  
FPD & Optoelectronics Show 2006
[19.05.2006]  
Metallurgy Litmash 2006
[10.05.2006]  
"PLANSEE inside"
[24.03.2006]  
SEMICON China 2006
[07.03.2006]  
Change of PLANSEE GmbH to PLANSEE SE
[21.02.2006]  
PLANSEE at SEMICON Korea 2006
[20.01.2006]  
STC certified to aerospace standards AS 9100
[22.12.2005]  
Organizational change at PLANSEE AG
[01.09.2005]  
PLANSEE supplies the violet part of the new bimetallic 25-Euro coin
[22.03.2005]  
Visit us at Glassman Europe 2005
[18.04.2005]  
PLANSEE starts operation of a new hot-forging machine
[06.09.2004]  
25 EURO Coin
[04.05.2004]  
PLANSEE Majority
[04.05.2004]  
 
Archive
Copyright 2010 PLANSEE SE    
All rights reserved.