Protective sheets for glass-melting tanks

[15/04/2009]

Corrosion-resistant molybdenum sheets help glass-melting tanks last longer, and improve glass quality.

Protective molybdenum sheets significantly reduce costly disruptions to the production process and time-consuming repairs – something product manager Heike Larcher knows to be one of the largest cost drivers in glass production. As a result, those who use protective sheets will see a quick return on their investment.
Heike Larcher explains: “Even when melting normal glass, the high temperatures can seriously corrode the refractory bricks used to build the furnace.” And these bricks are put under even greater strain when used to manufacture opal and pharmaceutical glass, as melting these products requires much higher temperatures. Molybdenum is much more corrosion-resistant than refractory bricks to many kinds of melted glass. As a result, it can be used to protect
the bricks from corrosion in particularly vulnerable areas. This extra reinforcement enables the bricks to keep their original size and shape for longer, which in turn leads to a higher quality of glass, and a longer life for the tank.
Because the molybdenum sheets must be built into the glass-melting tank when it is cold (i.e. before it is fired up for the first time), it is important to protect against oxidation as the tank slowly heats up. For this, Plansee has developed the SIBOR® coating for molybdenum – this guarantees complete protection against oxidization during this critical warmup phase. Additional protection against corrosion is offered by a special component used to protect the vulnerable corners of the throat. Plansee has now presented this solution to the public for the first time. The protective part reduces the danger of the melted glass getting behind the molybdenum plates.



 


Acquisition of Wolfra-Tech: PLANSEE strengthens activities in India
[08.07.2010]  
PLANSEE session at the ESG Conference
[10.06.2010]  
Meet our champion against corrosion
[27.05.2010]  
LED starts with a crucible
[28.04.2010]  
Bi-metal coin: Light as a feather and gleaming blue
[01.04.2010]  
A key component for high-temperature fuel cells
[24.03.2010]  
MoZrO2: Best in corrosion resistance
[23.03.2010]  
Furnace construction expertise for sapphire and silicon melting
[18.02.2010]  
MoZrO2 glass melting electrodes at the Glassman South America
[12.02.2010]  
New sputtering facility supports development of functional coatings
[08.02.2010]  
Multiple-parts solution for arc chambers
[08.02.2010]  
Refractory metals in the glass industry: PLANSEE session in Magdeburg
[03.02.2010]  
Flat screens for China.
[13.01.2010]  
One-stop shop for metallic sputtering targets
[19.11.2009]  
PLANSEE Powertech is preferred strategic supplier of Areva
[16.11.2009]  
Materials and Production Equipment for flat panel display technologies of tomorrow
[09.11.2009]  
Schedule of trade fairs 2009/10
[02.03.2009]  
On the Trail of Future Energy Trends: PLANSEE at international EGT congress
[05.11.2009]  
Direct sales of molybdenum spray wire
[30.10.2009]  
Meet our glass team in Dubai!
[28.10.2009]  
PLANSEE USA celebrates 70 years of business
[22.10.2009]  
Enhanced Glass Tank Performance
[20.10.2009]  
See you in Ohio! PLANSEE at the Glass Problems Conference
[07.10.2009]  
PLANSEE glass team on tour
[02.10.2009]  
Meet us at the PV Conference & Exhibition in Hamburg
[14.09.2009]  
Monolithic rotary sputtering targets
[21.08.2009]  
Plansee Group increases sales in the last fiscal year
[09.07.2009]  
Shaping the future development of growth industries
[25.05.2009]  
17 Plansee Seminar: „Innovation as a basis for future growth”
[25.05.2009]  
Protective sheets for glass-melting tanks
[15.04.2009]  
Sustainable collaboration
[03.04.2009]  
World's largest HIP cyclinder
[20.03.2009]  
Powder Metal community gathers in Reutte
[18.02.2009]  
Covering the entire coatings market
[15.12.2008]  
Plansee Group continues to grow: Sales reach over one billion euros for first time ever
[03.07.2008]  
Plansee Group acquires US powder expert GTP
[23.04.2008]  
The fascination of light: the core for the new 25 Euro coin from PLANSEE
[08.04.2008]  
Schedule of trade fairs 2008/09
[25.03.2008]  
Elektro-Metall becomes PLANSEE Powertech
[12.10.2007]  
Impressing result seen after shut down of a glass tank
[26.11.2007]  
FPD International 2007
[24.10.2007]  
V2007 Vakuumbeschichtung und Plasmaoberflächentechnik
[16.10.2007]  
PLANSEE continues to expand its international presence
[02.03.2007]  
New bimetallic 25-Euro coin - PLANSEE producing the turquoise niobium core
[20.03.2007]  
Plansee Group strengthens its position in North America
[01.12.2006]  
Mathematical simulation for glass tank reinforcements
[21.11.2006]  
PLANSEE with new corporate appearence
[18.09.2006]  
PLANSEE sponsors IIT2006 conference
[29.05.2006]  
FPD & Optoelectronics Show 2006
[19.05.2006]  
Metallurgy Litmash 2006
[10.05.2006]  
"PLANSEE inside"
[24.03.2006]  
SEMICON China 2006
[07.03.2006]  
Change of PLANSEE GmbH to PLANSEE SE
[21.02.2006]  
PLANSEE at SEMICON Korea 2006
[20.01.2006]  
STC certified to aerospace standards AS 9100
[22.12.2005]  
Organizational change at PLANSEE AG
[01.09.2005]  
PLANSEE supplies the violet part of the new bimetallic 25-Euro coin
[22.03.2005]  
Visit us at Glassman Europe 2005
[18.04.2005]  
PLANSEE starts operation of a new hot-forging machine
[06.09.2004]  
25 EURO Coin
[04.05.2004]  
PLANSEE Majority
[04.05.2004]  
 
Archive
Copyright 2010 PLANSEE SE    
All rights reserved.