Monolithic rotary sputtering targets

[21/08/2009]

Optimized sputtering processes significantly contribute to the efficient production of solar cells. Maximum material utilization, faster processes and top quality are key success factors for this industry. With its molybdenum monolithic rotary sputtering targets, PLANSEE fulfills these requirements and sets new standards for efficient coating. The targets will be presented in September at the Photovoltaic Solar Energy Conference in Hamburg/Germany.

As the leading supplier of planar and rotary sputtering targets for thin-film solar cells and flat panel displays, PLANSEE is continually developing innovative solutions for optimal sputtering results and an efficient coating process. For the photovoltaic industry the company now offers monolithic rotary targets made of 100 % molybdenum. Their design without a backing tube pays off: hundreds of tests have already proven the benefits in practice.

Fast process. High power. Maximum yield.
Without a low-melting bonding layer, monolithic targets allow the highest heat transfer rates. Monolithic rotary targets can be run with up to 30 kW/ m power. The advantage: greater productivity and improved efficiency for a faster coating process.

In general, rotary targets have double or even triple the material utilization of planar targets. The rotary monolithic versions hold the record: they maintain their stability even after target utilization of more than 75 %. Producers thereby profit from bigger production runs.

The manufacturing of monolithic targets is carried out without any bonding. This lean process implies a fast production and maximum cost efficiency for customers.

Fully densified materials for maximum solar cell efficiency
In cooperation with all major solar cell manufacturers, PLANSEE has developed new materials that improve the performance of the thin film absorber layers. By alloying and developing material compounds, PLANSEE adapts inherent material properties to meet the specific requirements of the customers and tune the chemical composition of thin film absorbers. For the solar industry, the company offers materials such as Mo, Cr, MoNa, CuGa, CuIn or CuInGa.

With its complete in-house manufacturing, extensive expertise in powder metallurgy and cutting-edge deformation technologies, PLANSEE guarantees the best quality materials for the coating industry. They stand out for their full density, high purity and a uniform and fine grained microstructure. For its molybdenum targets the company delivers an actual chemical analysis for 21 elements confirmed in a 3.1 certificate.

The company will present its latest developments for the solar industry at the 24th European Photovoltaic Solar Energy Conference & Exhibition in Hamburg (Sept. 21-25 2009).



 


Acquisition of Wolfra-Tech: PLANSEE strengthens activities in India
[08.07.2010]  
PLANSEE session at the ESG Conference
[10.06.2010]  
Meet our champion against corrosion
[27.05.2010]  
LED starts with a crucible
[28.04.2010]  
Bi-metal coin: Light as a feather and gleaming blue
[01.04.2010]  
A key component for high-temperature fuel cells
[24.03.2010]  
MoZrO2: Best in corrosion resistance
[23.03.2010]  
Furnace construction expertise for sapphire and silicon melting
[18.02.2010]  
MoZrO2 glass melting electrodes at the Glassman South America
[12.02.2010]  
New sputtering facility supports development of functional coatings
[08.02.2010]  
Multiple-parts solution for arc chambers
[08.02.2010]  
Refractory metals in the glass industry: PLANSEE session in Magdeburg
[03.02.2010]  
Flat screens for China.
[13.01.2010]  
One-stop shop for metallic sputtering targets
[19.11.2009]  
PLANSEE Powertech is preferred strategic supplier of Areva
[16.11.2009]  
Materials and Production Equipment for flat panel display technologies of tomorrow
[09.11.2009]  
Schedule of trade fairs 2009/10
[02.03.2009]  
On the Trail of Future Energy Trends: PLANSEE at international EGT congress
[05.11.2009]  
Direct sales of molybdenum spray wire
[30.10.2009]  
Meet our glass team in Dubai!
[28.10.2009]  
PLANSEE USA celebrates 70 years of business
[22.10.2009]  
Enhanced Glass Tank Performance
[20.10.2009]  
See you in Ohio! PLANSEE at the Glass Problems Conference
[07.10.2009]  
PLANSEE glass team on tour
[02.10.2009]  
Meet us at the PV Conference & Exhibition in Hamburg
[14.09.2009]  
Monolithic rotary sputtering targets
[21.08.2009]  
Plansee Group increases sales in the last fiscal year
[09.07.2009]  
Shaping the future development of growth industries
[25.05.2009]  
17 Plansee Seminar: „Innovation as a basis for future growth”
[25.05.2009]  
Protective sheets for glass-melting tanks
[15.04.2009]  
Sustainable collaboration
[03.04.2009]  
World's largest HIP cyclinder
[20.03.2009]  
Powder Metal community gathers in Reutte
[18.02.2009]  
Covering the entire coatings market
[15.12.2008]  
Plansee Group continues to grow: Sales reach over one billion euros for first time ever
[03.07.2008]  
Plansee Group acquires US powder expert GTP
[23.04.2008]  
The fascination of light: the core for the new 25 Euro coin from PLANSEE
[08.04.2008]  
Schedule of trade fairs 2008/09
[25.03.2008]  
Elektro-Metall becomes PLANSEE Powertech
[12.10.2007]  
Impressing result seen after shut down of a glass tank
[26.11.2007]  
FPD International 2007
[24.10.2007]  
V2007 Vakuumbeschichtung und Plasmaoberflächentechnik
[16.10.2007]  
PLANSEE continues to expand its international presence
[02.03.2007]  
New bimetallic 25-Euro coin - PLANSEE producing the turquoise niobium core
[20.03.2007]  
Plansee Group strengthens its position in North America
[01.12.2006]  
Mathematical simulation for glass tank reinforcements
[21.11.2006]  
PLANSEE with new corporate appearence
[18.09.2006]  
PLANSEE sponsors IIT2006 conference
[29.05.2006]  
FPD & Optoelectronics Show 2006
[19.05.2006]  
Metallurgy Litmash 2006
[10.05.2006]  
"PLANSEE inside"
[24.03.2006]  
SEMICON China 2006
[07.03.2006]  
Change of PLANSEE GmbH to PLANSEE SE
[21.02.2006]  
PLANSEE at SEMICON Korea 2006
[20.01.2006]  
STC certified to aerospace standards AS 9100
[22.12.2005]  
Organizational change at PLANSEE AG
[01.09.2005]  
PLANSEE supplies the violet part of the new bimetallic 25-Euro coin
[22.03.2005]  
Visit us at Glassman Europe 2005
[18.04.2005]  
PLANSEE starts operation of a new hot-forging machine
[06.09.2004]  
25 EURO Coin
[04.05.2004]  
PLANSEE Majority
[04.05.2004]  
 
Archive
Copyright 2010 PLANSEE SE    
All rights reserved.