As of 1 January 2010, PLANSEE Metall GmbH will take over responsibility for supplying customers with high-grade molybdenum spray wire from Sulzer Metco. As far as the customers are concerned, the only change is the point of contact, as Sulzer Metco had always sourced molybdenum spray wire exclusively from PLANSEE.
In the first half of 2009, Sulzer Metco had taken the decision to stop selling molybdenum spray wire in the light of increased competition and the volatility of the raw materials markets. Michael Androsch, responsible for sales and marketing of molybdenum spray wire at PLANSEE Metall, says: “Customers can continue to rely on first-class service from a global sales team, on high quality products and absolutely reliable delivery, just as they always could with Sulzer Metco.”
Molybdenum spray wire from PLANSEE is manufactured in state-of-the-art facilities in Reutte/Austria and is 100 % eddy-current tested. Its quality characteristics include a high degree of purity, consistent diameter and freedom from cracks. To guarantee security of supply, PLANSEE can manufacture its spray wire in a second plant in the United States.