| mat.no | dia [mm] | tol [mm] | quality | surface | approx weight [kg/1000 m] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] | standard spool |
| | | 332249 | 0.40 | +/- 0.008 | annealed | electropolished | 1.282 | 40 | 150 | 5 | SH253K | | 332240 | 0.50 | +/- 0.010 | annealed | electropolished | 2.003 | 40 | 150 | 10 | SD300K | | 327698 | 0.60 | +/- 0.012 | annealed | electropolished | 2.884 | 100 | 300 | 10 | SD300K | | 331052 | 0.70 | +/- 0.014 | annealed | electropolished | 3.923 | 100 | 200 | 10 | SD300K | | 332235 | 0.80 | +/- 0.012 | annealed | electropolished | 5.127 | 100 | 300 | 10 | SD300K | |