MLR - SHEETS
 
according to specification PS-GF026
RECRYSTALLIZED
RECRYSTALLIZED, HOT ROLLED, FINISHED CUT
 

mat.no thickness
[mm]
tol
[mm]
width
[mm]
tol
[mm]
length
[mm]
tol
[mm]
quality flatness
in %
approx
weight
[kg/pce]
quan.x
[kg]
lot size
[kg]
min.quant.
intermediate
sizes [kg]
 
285085 1.500 +/- 0.130 500.0 +/- 0.70 1200 +5/-0 hot rolled, pickled <1% 9.180 20 143 50
285014 2.000 +/- 0.150 500.0 +/- 0.70 1200 +5/-0 hot rolled, pickled <1% 12.240 25 143 50
284930 2.540 +/- 0.180 500.0 +/- 0.80 1200 +5/-0 hot rolled, pickled <1% 15.545 50 143 50
284920 3.175 +/- 0.180 500.0 +/- 2.00 1200 +5/-0 hot rolled, pickled <1% 19.431 50 143 50


   