| mat.no | thickness [mm] | tol [mm] | width [mm] | tol [mm] | length [mm] | tol [mm] | quality | flatness in % | approx weight [kg/pce] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 292645 | 0.200 | +/- 0.020 | 500.0 | +/- 0.50 | 1200 | +5/-0 | cold rolled, pickled | <1% | 1.224 | 20 | 72 | 50 | | 292640 | 0.300 | +/- 0.020 | 500.0 | +/- 0.50 | 1200 | +5/-0 | cold rolled, pickled | <1% | 1.836 | 30 | 69 | 50 | | 291748 | 0.500 | +/- 0.035 | 500.0 | +/- 0.60 | 1200 | +5/-0 | cold rolled, pickled | <1% | 3.060 | 30 | 93 | 50 | | 11012259 | 1.000 | +/- 0.035 | 500.0 | +/- 0.60 | 1200 | +5/-0 | cold rolled, pickled | <1% | 6.120 | 30 | 147 | 50 | |