| mat.no | dia [mm] | tol [mm] | length [mm] | quality | straight- ness [per m] | approx weight [kg/m] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 104602 | 31.75 | +/- 0.300 | 1000 - 2000 | smooth forged | <2.0 | 8.100 | 80 | 600 | 600 | | 105301 | 48.00 | +/- 0.300 | 800 - 1600 | smooth forged | <1.5 | 18.500 | 160 | 400 | 400 | | 160717 | 50.80 | +0.000/-0.800 | 1000 - 2000 | smooth forged | <1.0 | 20.700 | 300 | 450 | 450 | | 105324 | 54.00 | +/- 0.400 | 1000 - 2000 | smooth forged | <1.0 | 23.400 | 50 | 400 | 400 | | 105325 | 60.00 | +/- 0.400 | 1000 - 2000 | smooth forged | <1.0 | 28.800 | 100 | 500 | 500 | | 105331 | 63.50 | +/- 0.400 | 1000 - 2000 | smooth forged | <1.0 | 32.300 | 200 | 500 | 500 | | 233494 | 66.00 | +/- 0.400 | 1000 - 2000 | smooth forged | <1.0 | 34.900 | 120 | 500 | 500 | | 105334 | 70.00 | +/- 0.400 | 1000 - 2000 | smooth forged | <2.5 | 39.300 | 120 | 500 | 500 | | 105450 | 76.20 | +/- 1.000 | 1000 - 2000 | smooth forged | <2.5 | 46.500 | 120 | 450 | 450 | | 11387513 | 79.00 | +/- 1.000 | 1000 - 2000 | smooth forged | <2.5 | 50.000 | 80 | 500 | 500 | | 105452 | 80.00 | +/- 1.000 | 1000 - 2000 | smooth forged | <2.5 | 51.300 | 80 | 500 | 500 | | 105457 | 90.00 | +/- 1.000 | 1000 - 2000 | smooth forged | <2.5 | 64.900 | 80 | 500 | 500 | | 105467 | 101.20 | +/- 1.000 | 1000 - 2000 | smooth forged | <2.5 | 82.000 | 200 | 500 | 500 | standard threads | | M 18 x 1.5 | | M 22 x 1.5 | | M 24 x 1.5 | | M 27 | | M 36 x 3 | | M 42 x 3 | |
| |