| mat.no | thickness [mm] | tol [mm] | width [mm] | tol [mm] | length [mm] | tol [mm] | quality | flatness in % | approx weight [kg/pce] | quan.x [kg] | lot size [kg] | pcs.per packing unit | min.quant. intermediate sizes [kg] |
| | | 264393 | 0.127 | +/- 0.015 | 609.6 | +/- 0.50 | 2000 | +5/-0 | cold rolled, pickled | <1% | 1.579 | 15 | 151 | 12 | 50 | | 11011420 | 0.200 | +/- 0.020 | 600.0 | +/- 0.50 | 2000 | +5/-0 | cold rolled, bright | <1% | 2.448 | 20 | 137 | 6 | 50 | | 257106 | 0.200 | +/- 0.020 | 600.0 | +/- 0.50 | 2000 | +5/-0 | cold rolled, pickled | <1% | 2.448 | 25 | 137 | 6 | 50 | | 264409 | 0.254 | +/- 0.020 | 609.6 | +/- 0.50 | 2000 | +5/-0 | cold rolled, pickled | <1% | 3.159 | 25 | 173 | 6 | 50 | | 11011421 | 0.300 | +/- 0.020 | 600.0 | +/- 0.50 | 2000 | +5/-0 | cold rolled, bright | <1% | 3.672 | 20 | 205 | 6 | 50 | | 257117 | 0.300 | +/- 0.020 | 600.0 | +/- 0.50 | 2000 | +5/-0 | cold rolled, pickled | <1% | 3.672 | 50 | 205 | 6 | 50 | | 264415 | 0.381 | +/- 0.030 | 609.6 | +/- 0.50 | 2000 | +5/-0 | cold rolled, pickled | <1% | 4.738 | 20 | 211 | 6 | 50 | | 11012258 | 0.500 | +/- 0.035 | 600.0 | +/- 0.60 | 2000 | +5/-0 | cold rolled, bright | <1% | 6.120 | 30 | 342 | 3 | 50 | | 257246 | 0.500 | +/- 0.035 | 600.0 | +/- 0.60 | 2000 | +5/-0 | cold rolled, pickled | <1% | 6.120 | 200 | 342 | 3 | 50 | | 11012096 | 1.000 | +/- 0.040 | 600.0 | +/- 0.60 | 2000 | +5/-0 | cold rolled, bright | <1% | 12.240 | 60 | 367 | 1 | 50 | | 257249 | 1.000 | +/- 0.040 | 600.0 | +/- 0.60 | 2000 | +5/-0 | cold rolled, pickled | <1% | 12.240 | 60 | 367 | 1 | 50 | | 257308 | 1.500 | +/- 0.060 | 600.0 | +/- 0.80 | 2000 | +5/-0 | cold rolled, pickled | <1% | 18.360 | 75 | 385 | 1 | 50 | | 289513 | 2.000 | +/- 0.150 | 500.0 | +/- 0.70 | 1000 | +5/-0 | hot rolled, pickled | <1% | 10.200 | 40 | 370 | 0 | 50 | | 289516 | 3.000 | +/- 0.180 | 500.0 | +/- 0.80 | 1000 | +5/-0 | hot rolled, pickled | <1% | 15.300 | 60 | 379 | 0 | 50 | | 284145 | 5.000 | +/- 0.250 | 500.0 | +/- 2.00 | 1000 | +5/-0 | hot rolled, pickled | <1% | 25.500 | 60 | 265 | 0 | 50 | | 284171 | 6.000 | +/- 0.300 | 500.0 | +/- 2.40 | 850 | +5/-0 | hot rolled, pickled | <1% | 26.010 | 30 | 265 | 0 | 50 | | 11011391 | 7.000 | +/- 0.350 | 500.0 | +/- 2.80 | 750 | +5/-0 | hot rolled, pickled | <1% | 26.775 | 30 | 265 | 0 | 50 | | 11011405 | 8.000 | +/- 0.400 | 500.0 | +/- 2.80 | 650 | +5/-0 | hot rolled, pickled | <1% | 26.520 | 30 | 265 | 0 | 50 | | 284323 | 10.000 | +/- 0.500 | 500.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 30.600 | 100 | 678 | 0 | 90 | | 284330 | 12.700 | +/- 0.630 | 400.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 31.090 | 60 | 678 | 0 | 90 | | 284331 | 20.000 | +/- 1.000 | 400.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 48.960 | 100 | 678 | 0 | 180 | | 284333 | 30.000 | +/- 1.500 | 400.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 73.440 | 80 | 678 | 0 | 180 | | 284377 | 40.000 | +/- 2.000 | 400.0 | +/- 2.00 | 500 | +5/-0 | hot rolled, pickled | <1% | 81.600 | 160 | 712 | 0 | 250 | |