MO - SPRAY_WIRE
 
according to specification PS-HPR114
 

mat.no dia
[mm]
tol
[mm]
quality approx
weight
[kg/1000 m]
quan.x
[kg]
lot size
[kg]
min.quant.
intermediate
sizes [kg]
 
190524 2.31 +/- 0.025 black, 8 - 13 kg 42.748 500 800 0
6305 2.31 +/- 0.025 black, 18 - 24 kg 42.748 500 800 0
190507 3.17 +0.000/-0.050 black, 10 - 13 kg 80.502 500 800 0
6306 3.17 +0.000/-0.050 black, 18 - 24 kg 80.502 500 800 0


   