| mat.no | dia [mm] | tol [mm] | quality | surface | approx weight [kg/1000 m] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 15903 | 0.50 | +/- 0.010 | annealed | electropolished | 2.003 | 10 | 50 | 10 | | 150532 | 1.00 | +/- 0.015 | annealed | electropolished | 8.011 | 20 | 100 | 10 | | 137259 | 2.00 | +/- 0.020 | annealed | pickled | 32.044 | 15 | 100 | 10 | | 128644 | 2.50 | +/- 0.025 | annealed | pickled | 50.069 | 20 | 100 | 10 | | 149948 | 3.00 | +/- 0.030 | annealed | pickled | 72.100 | 25 | 100 | 10 | |