| mat.no | thickness [mm] | tol [mm] | width [mm] | tol [mm] | approx weight [kg/1000 m] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 306922 | 0.020 | +0.003/-0.002 | 1.5 | +/- 0.10 | 0.230 | 2 | 5 | 2 | | 280570 | 0.025 | +0.003/-0.002 | 2.0 | +/- 0.10 | 0.383 | 2 | 5 | 2 | | 289972 | 0.025 | +0.003/-0.002 | 2.5 | +/- 0.10 | 0.491 | 2 | 5 | 2 | | 280520 | 0.025 | +0.003/-0.002 | 3.0 | +/- 0.20 | 0.574 | 2 | 5 | 2 | | 289781 | 0.025 | +0.003/-0.002 | 4.0 | +/- 0.20 | 0.765 | 2 | 5 | 2 | | 289774 | 0.028 | +0.003/-0.002 | 2.0 | +/- 0.10 | 0.428 | 2 | 5 | 2 | | 289775 | 0.028 | +0.003/-0.002 | 2.5 | +/- 0.10 | 0.536 | 2 | 5 | 2 | | 286163 | 0.028 | +0.003/-0.002 | 3.0 | +/- 0.20 | 0.643 | 2 | 5 | 2 | | 289993 | 0.028 | +0.003/-0.002 | 4.0 | +/- 0.20 | 0.857 | 2 | 5 | 2 | | 279534 | 0.030 | +0.004/-0.003 | 3.0 | +/- 0.20 | 0.689 | 2 | 5 | 2 | | 289974 | 0.035 | +0.004/-0.003 | 6.0 | +/- 0.30 | 1.607 | 2 | 5 | 2 | | 291771 | 0.040 | +0.004/-0.003 | 10.0 | +/- 0.40 | 3.040 | 2 | 5 | 2 | |