| mat.no | thickness [mm] | tol [mm] | width [mm] | tol [mm] | length [mm] | tol [mm] | quality | flatness in % | approx weight [kg/pce] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 140760 | 1.000 | +/- 0.080 | 600.0 | +/- 0.60 | 2000 | +5/-0 | hot rolled, pickled | <1% | 12.180 | 15 | 250 | 50 | | 209630 | 1.500 | +/- 0.130 | 600.0 | +/- 0.80 | 2000 | +5/-0 | hot rolled, pickled | <1% | 18.270 | 20 | 376 | 50 | | 209633 | 2.000 | +/- 0.150 | 600.0 | +/- 0.80 | 2000 | +5/-0 | hot rolled, pickled | <1% | 24.360 | 30 | 400 | 50 | | 210547 | 2.500 | +/- 0.180 | 600.0 | +/- 1.00 | 2000 | +5/-0 | hot rolled, pickled | <1% | 30.450 | 35 | 500 | 50 | | 210528 | 3.000 | +/- 0.180 | 600.0 | +/- 1.00 | 2000 | +5/-0 | hot rolled, pickled | <1% | 36.720 | 37 | 752 | 50 | | 321572 | 5.000 | +/- 0.250 | 500.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 15.225 | 30 | 180 | 50 | | 321638 | 10.000 | +/- 0.500 | 400.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 24.360 | 30 | 360 | 360 | | 321607 | 20.000 | +/- 1.000 | 400.0 | +/- 2.00 | 600 | +5/-0 | hot rolled, pickled | <1% | 48.720 | 50 | 360 | 360 | |