| mat.no | thickness [mm] | tol [mm] | width [mm] | tol [mm] | length [mm] | tol [mm] | quality | flatness in % | approx weight [kg/pce] | quan.x [kg] | lot size [kg] | pcs.per packing unit |
| | | 11213205 | 0.500 | +/- 0.110 | 500.0 | +/- 1.20 | 1000 | +5/-0 | hot rolled, pickled | <1% | 4.825 | 30 | 216 | 3 | | 11213212 | 1.000 | +/- 0.200 | 500.0 | +/- 1.20 | 1000 | +5/-0 | hot rolled, pickled | <1% | 9.650 | 60 | 240 | 1 | | 11213315 | 1.500 | +/- 0.250 | 500.0 | +/- 1.70 | 1000 | +5/-0 | hot rolled, pickled | <1% | 14.475 | 35 | 240 | 1 | | 11213317 | 2.000 | +/- 0.250 | 500.0 | +/- 1.70 | 1000 | +5/-0 | hot rolled, pickled | <1% | 19.300 | 40 | 248 | 1 | | 11213321 | 3.000 | +/- 0.300 | 300.0 | +/- 1.70 | 800 | +5/-0 | hot rolled, pickled | <1% | 13.896 | 25 | 128 | 1 | | 11213323 | 4.000 | +/- 0.200 | 200.0 | +/- 1.70 | 600 | +5/-0 | hot rolled, pickled | <1% | 9.264 | 30 | 126 | 1 | | 11213326 | 5.000 | +/- 0.200 | 200.0 | +/- 1.70 | 550 | +5/-0 | hot rolled, pickled | <1% | 10.615 | 35 | 144 | 1 | |