| mat.no | dia [mm] | tol [mm] | length [mm] | quality | straight- ness [per m] | rough- ness (Ra) | approx weight [kg/m] | quan.x [kg] | lot size [kg] | min.quant. intermediate sizes [kg] |
| | | 11239686 | 3.50 | +/- 0.015 | 700 - 2100 | ground | <2.5 | <0.4 | 0.186 | 10 | 50 | 10 | | 11239689 | 4.50 | +/- 0.015 | 700 - 2100 | ground | <2.5 | <0.4 | 0.307 | 15 | 50 | 20 | | 11239705 | 5.50 | +/- 0.015 | 700 - 2100 | ground | <2.5 | <0.4 | 0.458 | 10 | 60 | 20 | | 11239707 | 6.00 | +/- 0.015 | 700 - 2100 | ground | <2.5 | <0.4 | 0.545 | 15 | 30 | 20 | | 11239708 | 6.50 | +/- 0.015 | 700 - 2100 | ground | <2.5 | <0.4 | 0.640 | 15 | 30 | 20 | | 11239719 | 7.00 | +/- 0.020 | 700 - 2100 | ground | <2.5 | <0.4 | 0.742 | 20 | 50 | 20 | | 11239722 | 9.00 | +/- 0.020 | 700 - 2100 | ground | <2.5 | <0.4 | 1.227 | 20 | 50 | 20 | | 273299 | 40.00 | +/- 0.400 | 500 - 2800 | forged | <1.5 | | 24.241 | 50 | 265 | 200 | | 262137 | 45.00 | +/- 0.500 | 500 - 2100 | forged | <1.5 | | 30.680 | 30 | 265 | 210 | | 279098 | 60.00 | +/- 0.500 | 500 - 2500 | forged | <1.5 | | 54.542 | 60 | 225 | 210 | | 268387 | 80.00 | +/- 1.000 | 500 - 1500 | forged | <2.0 | | 96.963 | 60 | 275 | 135 | |