WVM - WIRE
 
according to specification PS-GR103
 

mat.no dia
[mm]
tol
[mm]
quality surface approx
weight
[kg/1000 m]
quan.x
[kg]
lot size
[kg]
min.quant.
intermediate
sizes [kg]
 
256123 0.64 +/- 0.013 cleaned, unannealed pickled 6.112 15 80 5
128489 0.76 +/- 0.011 cleaned, unannealed pickled 8.755 15 80 5
9157 1.00 +/- 0.015 cleaned, unannealed pickled 15.158 15 80 5


   