Centreless grinding
Through-feed grinding, diameter range 3.0 - 10.0 mm;
Plunge-cut grinding, diameter range 0.1 - 1.0 mm
-
Turning
small components -diameter to 0.5 mm; large components up to 700 mm diameter
-
Milling
Complex 3D forms (including programming)
-
Wire erosion
Workpiece sizes up to 600 mm length, 100 mm width
-
Spark erosion
for producing pilot holes
-
Laser cutting
Sheet section up to 800 mm x 1000 mm, thickness up to 6 mm
-
Laser marking
of finished components
-
Laser structure modification
Development of complex surface structures on finished parts
-
Photoetching
Production of complex forms in refractory metals up to 0.3 mm thickness
-
Electropolishing
small components up to 10 mm x 10 mm, large components (crucibles) up to 400 mm diameter x 400 mm high
-
Deep-hole boring
Diameter 2.0 - 50.0 mm, depth up to 2000 mm
-
Galvanic coating
including vacuum annealing capability
-
Plasma coating
round and flat components, sheets 1000 mm x 3000 mm
-
Water-jet cutting
Sheet section up to 800 mm x 1000 mm, thickness up to 30 mm
-
Pressing
Titanium/Aluminium parts in diameter range 30 - 80 mm, thickness up to 40 mm
-
Filament winding
Mass production as well as small runs
-
Brazing
-
Pressing
of large components
-
Precision rod grinding
including holding and measuring tolerances of 0.5 µm
-
Coining
of parts up to 30 mm x 150 mm, thickness up to 0.5 mm
-
Friction welding
of copper, molybdenum, steel
-
Electron beam welding
-
Pin grinding
Diameter range 0.1 to 1 mm, length from 10 to 200 mm
-
Stamping
Foils and sheets from 0.05 mm to 1.0 mm, finished parts 50 mm x 50 mm, washers 2000 mm OD x 1000 mm ID x 2 mm
-
Cutting
Pins and rods, diameter range 0.3 mm to 5.0 mm with lengths 1.0 mm - 20 mm
-
Wire mesh
Wire mesh DIN 4189 / Opening 0.5, wire diameter 0.2 / 2500 x 2000 mm
-
Tube bending
Spirals and special forms