Part of a Multi-Leaf Collimator Worldwide DENSIMET alloys have for years been used successfully for protection against natural and artificial radiation.
Most common applications for these PLANSEE alloys are their use in radiation devices for therapie as well as for diagnosis: Shieldings protect from uncontrolled radiation leakage. Collimators guide, form and focus radiation. Containers made from DENSIMET are very often used to protect Isotopes during transportation and storage.

Advantages:

  • High density 
  • High absorption of gamma and X- rays
  • Good machinability
  • Environmentally friendly

Forms of delivery:

Finished products: 

  • Production according to customer drawings

Semi-finished products from stock: 

  • Rods up to 62 mm dia
  • Plates up to max. 60 x 160 x 400 mm
  • Larger dimensions upon request