In resistance welding, tungsten and molybdenum based welding electrodes win you over with their longevity.
PLANSEE welding electrode made of tungsten and molybdenum are electrodes are especially suitable for the welding of metals with high electrical conductivity such as copper and silver. They are used in the following welding processes:
-
Spot-welding
-
Roller-welding
-
Projection-welding
-
Upset butt welding
|
Our materials for resistance welding |
| |
Composition |
Density g / cm3 |
Hardness HV 10 |
Electrical Conductivity m/Omm2 |
Thermal conductivity W/m°C |
Recrystallization temperature °C |
|
Molybdenum |
Mo min. 99.97 % |
10.2 |
220-300 |
19 |
140 |
900-1100 |
|
TZM |
Mo = 99.3 % (min.) Ti = 0.5 % Zr = 0.08 % C = 0.01-0.04 % |
10.2 |
240-320 |
15 |
126 |
1300-1400 |
|
MHC |
Mo = 98.7 % Hf = 1.2 % C = 0.1 % |
10.2 |
270-320 |
14 |
110 |
1300-1450 |
|
Tungsten |
W min 99.97 % |
19.3 |
420-500 |
18 |
164 |
1200-1350 |
|
Thoriated tungsten |
W = 98 % ThO2 = 2 % |
19.3 |
450-500 |
approx. 17 |
approx. 150 |
> 1500 |
|
ELMET K 20N |
W = 80 % Cu = 20 % |
15.6 |
200-240 |
approx. 16 |
126 |
> 1000 |
|
DENSIMET D18 |
W = 95 % Fe = 1.6 % Ni = 3.4 % |
18.0 |
300-340 |
approx. 8 |
ca. 70 |
> 1000 |
|
ELMET E |
Cu = 99.5 % Cr = 0.4 % Zr = 0.1 % |
8-9 |
155-175 |
46-48 |
ca. 320 |
ca. 500 |
|
SPARKAL® X |
W = 75 % Cu = 25 % |
14.8 |
240 |
40 |
215 |
|
Questions about materials and design? You are in the right place.
We are happy to advise you personally on which material is suitable for your particular application area. With our experience in the processing of refractory materials, we also adapt the design of our welding electrodes to fit your specific application. In addition to finished/manufactured electrodes, PLANSEE also provides blanks for further processing.