Stirrers for Homogenising and Portioning

coated stirrers for homogenising glass melts

Stirring tools made of molybdenum are used both for the homogenising and for the portioning of glass melts. In addition we offer highly creep resistant stirrer shafts made of TZM and MoW.

In many cases the stirrers are either completely or partially clad with Platinum.

 

 

 

These metal stirrers offer the following advantages compared with conventional ceramic stirrers

  • Better stirring effect due to unlimited geometrical design possibilities
  • Higher mechanical strength and thermal shock resistance
  • No contamination of the glass melt
  • Longer service life

 

Compared with hollow platinum stirrers, stirring tools from PLANSEE offer the following advantages:

  • Lower investment costs
  • Higher strength

 

Advantages:

  • One source from the semi-finished part right through to the diffusion protection barrier
  • Economical manufacture due to the in-house production of pre-material
  • Outgas tested pre-material
  • Testing for cracks by means of ultrasound and die penetrant tests
  • Outgas certificate available upon customer request
  • Comprehensive advice and a wide range of available material and stirrer design solutions
  • Availability of computer modelling and subsequent design optimisation

 

Product Description:

Mill Products:

  • Rods, Discs, Sheets made of refractory metals

Finished Products:

  • Portioning and homogenising stirrers made of Mo, TZM, Mo/W in accordance with customer drawing or PLANSEE design recommendation
  • Platinum-clad stirrers according to customer drawing completed together with our partners in the platinum industry
  • All stirring tools available with ceramic diffusion barrier coating upon customer request

 

For further information please contact our glass team.



Sputtering targets for hard coating at the AMB in Stuttgart. Join us!
[08.09.2010]  
PLANSEE Hochleistungswerkstoffe startet Online-Shop
[06.09.2010]  
TiB2 sputtering targets for hard coating at the PSE conference
[06.09.2010]  
Acquisition of Wolfra-Tech: PLANSEE strengthens activities in India
[08.07.2010]  
PLANSEE session at the ESG Conference
[10.06.2010]  
 
Archive
Copyright 2010 PLANSEE SE    
All rights reserved.