X-ray targets can be subjected to higher loadings than stationary anodes. By rotation of dish-shaped X-ray targets under the electron beam, a new, already cooled part of the target surface is continually used as the focal spot. Moreover, the X-ray target cooles down more rapidly by radiating its heat. Far more energy per unit time can therefore be supplied to an X-ray tube with an X-ray target in comparison with a stationary anode.
 

 

 

 

 

Mammography X-ray Targets

Gentle X-ray radiation below 30 keV is required for mammography. X-ray targets made of molybdenum meet these requirements, because the peaks of the Ka- and Kb-lines of molybdenum are 17.5 and 19.65 keV and the emission is independent from the tube voltage.

 

Advantages:

  • PLANSEE supplies the whole range of Mo alloys which are optimally suited for individual customer requirements. 

 

Forms of delivery:

  • Molybenum X-ray targets according to customer specifications

 

 

Metal X-ray Targets
 

Metal X-ray targets are used in different areas of the modern x-ray technology: from the general medical diagnostic and angio- and cardiography to computer tomography.

 

Advantages:

  • As an independent supplier PLANSEE offers the complete range of metal X-ray targets. Experiences through the years and application know-how make us a specialist on that sector.

 

Forms of delivery:

  • RT-TZM targets (they have a TZM body, which imparts a greater resistance to warping under non-uniform heating)
  • RT-TZM targets with heat-emitting layers - for higher resistance
  • VPS-coated x-ray targets

 

 

Graphite backed X-ray targets

 

Graphite backed X-ray targets consist of a thin focal path of a tungsten-rhenium alloy with 5 or 10% rhenium, behind which is the TZM body. In turn it is brazed onto a layer of high purity graphite which varies in thickness.

 

The TZM body imparts outstanding dimensional stability under severe heating, whilst the graphite layer gives it a much higher heat capacity and a higher heat emission capacity. Because they can be subjected to high thermal stresses, the graphite backed X-ray targets  are particularly suitable for X-ray tubes  in computerised tomography as well as in the general medical diagnostic or in the angio- and cardiography.

 

Forms of delivery:

  • RT-TZM-C targets
  • coated graphite targets as per customer's drawings
  • X-ray targets with shaft or rotor according to customer's drawings

 

PLANSEE also supplies fastening systems and cathode components for various types of X-ray targets. 



How we influence the manufacturing costs and efficiency of CIGS.
[25.01.2012]  
Meet us in Tokyo and Santa Clara!
[13.01.2012]  
Plansee Group sells PMG
[16.12.2011]  
PLANSEE Express offers payment via PayPal
[01.12.2011]  
PLANSEE Tantalum Certified by EICC as „Conflict-Free“
[08.11.2011]  
PLANSEE grows in Korea
[24.10.2011]  
PLANSEE Express online shop opens for American and Canadian markets
[10.10.2011]  
New findings about Laser Structuring of Sputtered Molybdenum
[25.08.2011]  
And the Best Paper Award goes to: PLANSEE.
[18.08.2011]  
Sales increase by 46 percent: Plansee Group achieves best ever figures.
[07.07.2011]  
Blazing heat asks for solid components: PLANSEE at the Thermprocess 2011.
[22.06.2011]  
More efficiency: Molybdenum components for coating facilities.
[09.05.2011]  
Production site in Japan in full operation
[20.04.2011]  
Plansee Group acquires minority ownership of the Chilean company Molibdenos y Metales S.A.
[28.03.2011]  
Online shop now available throughout Europe
[07.02.2011]  
Meet our PVD Coating Team at the SVC in Chicago!
[27.01.2011]  
And the winner is: Multi-leaf collimators for targeted irradiation
[24.01.2011]  
Acquisition of Wolfra-Tech completed
[11.01.2011]  
The right tone - The Plansee wind orchestra released a new CD
[20.12.2010]  
World record with tungsten target
[24.11.2010]  
Revolution at 1,100 kV
[05.11.2010]  
Thorium-free TIG welding electrodes gain in popularity
[28.10.2010]  
On the trail of fine cracks: PLANSEE at the international powder metallurgy conference in Florence
[28.10.2010]  
Thank you for coming. When will we meet again?
[11.10.2010]  
Take the easy way: Sodium doped sputtering targets for CIS/CIGS solar cells.
[27.09.2010]  
Our champion against corrosion at the GLASSTEC. See you in the ring!
[23.09.2010]  
Get to know our strong metals at the ELMIA Subcontractor Show in Sweden
[14.09.2010]  
Sputtering targets for hard coating at the AMB in Stuttgart. Join us!
[08.09.2010]  
PLANSEE Hochleistungswerkstoffe startet Online-Shop
[06.09.2010]  
TiB2 sputtering targets for hard coating at the PSE conference
[06.09.2010]  
Acquisition of Wolfra-Tech: PLANSEE strengthens activities in India
[08.07.2010]  
PLANSEE session at the ESG Conference
[10.06.2010]  
Meet our champion against corrosion
[27.05.2010]  
LED starts with a crucible
[28.04.2010]  
Bi-metal coin: Light as a feather and gleaming blue
[01.04.2010]  
A key component for high-temperature fuel cells
[24.03.2010]  
MoZrO2: Best in corrosion resistance
[23.03.2010]  
Furnace construction expertise for sapphire and silicon melting
[18.02.2010]  
MoZrO2 glass melting electrodes at the Glassman South America
[12.02.2010]  
New sputtering facility supports development of functional coatings
[08.02.2010]  
Multiple-parts solution for arc chambers
[08.02.2010]  
Refractory metals in the glass industry: PLANSEE session in Magdeburg
[03.02.2010]  
Flat screens for China.
[13.01.2010]  
One-stop shop for metallic sputtering targets
[19.11.2009]  
PLANSEE Powertech is preferred strategic supplier of Areva
[16.11.2009]  
Materials and Production Equipment for flat panel display technologies of tomorrow
[09.11.2009]  
Schedule of trade fairs 2009/10
[02.03.2009]  
On the Trail of Future Energy Trends: PLANSEE at international EGT congress
[05.11.2009]  
Direct sales of molybdenum spray wire
[30.10.2009]  
Meet our glass team in Dubai!
[28.10.2009]  
PLANSEE USA celebrates 70 years of business
[22.10.2009]  
Enhanced Glass Tank Performance
[20.10.2009]  
See you in Ohio! PLANSEE at the Glass Problems Conference
[07.10.2009]  
PLANSEE glass team on tour
[02.10.2009]  
Meet us at the PV Conference & Exhibition in Hamburg
[14.09.2009]  
Monolithic rotary sputtering targets
[21.08.2009]  
Plansee Group increases sales in the last fiscal year
[09.07.2009]  
Shaping the future development of growth industries
[25.05.2009]  
17 Plansee Seminar: „Innovation as a basis for future growth”
[25.05.2009]  
Protective sheets for glass-melting tanks
[15.04.2009]  
Sustainable collaboration
[03.04.2009]  
World's largest HIP cyclinder
[20.03.2009]  
Powder Metal community gathers in Reutte
[18.02.2009]  
Covering the entire coatings market
[15.12.2008]  
Plansee Group continues to grow: Sales reach over one billion euros for first time ever
[03.07.2008]  
Plansee Group acquires US powder expert GTP
[23.04.2008]  
The fascination of light: the core for the new 25 Euro coin from PLANSEE
[08.04.2008]  
Schedule of trade fairs 2008/09
[25.03.2008]  
Elektro-Metall becomes PLANSEE Powertech
[12.10.2007]  
Impressing result seen after shut down of a glass tank
[26.11.2007]  
FPD International 2007
[24.10.2007]  
V2007 Vakuumbeschichtung und Plasmaoberflächentechnik
[16.10.2007]  
PLANSEE continues to expand its international presence
[02.03.2007]  
New bimetallic 25-Euro coin - PLANSEE producing the turquoise niobium core
[20.03.2007]  
Plansee Group strengthens its position in North America
[01.12.2006]  
Mathematical simulation for glass tank reinforcements
[21.11.2006]  
PLANSEE with new corporate appearence
[18.09.2006]  
PLANSEE sponsors IIT2006 conference
[29.05.2006]  
FPD & Optoelectronics Show 2006
[19.05.2006]  
Metallurgy Litmash 2006
[10.05.2006]  
"PLANSEE inside"
[24.03.2006]  
SEMICON China 2006
[07.03.2006]  
Change of PLANSEE GmbH to PLANSEE SE
[21.02.2006]  
PLANSEE at SEMICON Korea 2006
[20.01.2006]  
STC certified to aerospace standards AS 9100
[22.12.2005]  
Organizational change at PLANSEE AG
[01.09.2005]  
PLANSEE supplies the violet part of the new bimetallic 25-Euro coin
[22.03.2005]  
Visit us at Glassman Europe 2005
[18.04.2005]  
PLANSEE starts operation of a new hot-forging machine
[06.09.2004]  
25 EURO Coin
[04.05.2004]  
PLANSEE Majority
[04.05.2004]  
 
Archive
Copyright 2012 PLANSEE SE    
All rights reserved.