Back-cast
Back-cast materials simultaneously combine the material properties of two different material components. During this process, the materials themselves are retained in their original state and are bound only at a thin junction. The metals are fused in a mould to form a bond of only a few micrometres in size. Unlike welding and soldering techniques, this method is particularly stable and ensures optimum thermal conduction.