Basic hot zone for moderate operating conditions.

The basic version in our range of hot zones features a tried-and-tested standard design and uses standard materials (pure molybdenum and steel), making it the most affordable hot zone in the range. We manufacture our heating elements from ML, a molybdenum alloy that offers superb dimensional stability. Elements such as gas nozzles or offset shielding are available as options for the basic version.

We recommend our basic hot zone for temperatures up to 1,350 °C / 2,462 °F.

ML ribbon heating element with dual groove
Molybdenum support post and rail
Steel support frame

Find out more about the details and all the features of our different equipment packages:

We would be happy to draw up an individual estimate for you. Just let us know your requirements. You will receive a response from us within 48 hours.

Standard headline
Your contact Person for:
David Hoskins
Give me a call:
+1 508 446 5327
or send an Email:
david.hoskins@plansee.com