30/01/2025

From the concept to perfection: metal injection molding at Plansee

Using metal injection molding (MIM), Plansee can produce precise components with complex geometries and outstanding mechanical properties in quantities both small and large: efficiently, cost-effectively, and sustainably. From machining technology and medtech through to electronics, the safety industry, or sheet metal processing tools, metal injection molding is employed in a wide variety of industries. 

Discover why Plansee is the perfect partner for metal injection molding of refractory metals:

Creating the perfect component step by step

 

Production of the tool:

  • Feasibility study, design, and simulation using finite element method (FEM)
  • Tool production using modern equipment such as milling, eroding, and grinding machines or manual polishing

Production of the component:

  • Production of the feedstock
  • Injection molding process
  • Debinding and sintering
  • Quality control 
MIM

   

Discover the potential of metal injection molding at Plansee and be prepared to be amazed by our innovative power!