Reliable and durable: components for the telecommunications industry

Telecommunications is all about transmitting information via signals. The materials being used must meet the strictest requirements so that no information is lost even over long distances.

Our products are used to ensure reliable signal transmission in base stations, e.g., as base plates made of tungsten-copper (WCu). However, they also play an important role in smartphones, where they ensure that the signal with the information can be processed accordingly.

Our metals ensure sufficient cooling as base plates and heat spreaders, supporting the reliable transmission of information. As epitaxy process components for the core of telecommunications – chip manufacturing – they guarantee the sustainable function of semiconductor components.

Your advantages at a glance:

  • International production
    network

  • Wide-ranging product portfolio

  • Decades of application
    knowledge

  • Mass
    production
    capacities

  • Flexible production
    options

  • Highest product quality

Learn more about our products for telecommunications:

From powder to the final product

Thanks to our decades of experience, we can not only handle difficult-to-process materials, but also maintain the strictest tolerances. This guarantees precision. You will also profit from the decades of technical knowledge of our materials scientists and engineers. The same is true for our investment in mines in the West and our in-house production. A secure raw material supply and delivery capability as well as consistently high quality are thus guaranteed. Our continual investments in the latest facilities and machines enable us to provide high production capacities as well as the option for series and mass production. This makes us a flexible and reliable partner. And this has been true for one hundred years.

    Oxide
    Reduction
    Mixing alloys
    Pressing
    Sintering
    Forming
    Heat treatment
    Mech. processing
    Quality assurance
    Recycling
OxideMolymet (Chile) is the world's largest processor of molybdenum ore concentrates and our main supplier of molybdenum trioxide. The Plansee Group holds a 21.15% share in Molymet. Global Tungsten & Powders (USA) is a division of the Plansee Group and our main supplier of tungsten metal powder.