Raw materials are the future!

From the 1st of March through to the 31st of May 2016, the Montana University in Leoben will again be welcoming visitors to the "Rohstoffe sind Zukunft" exhibition.

The exhibition presents the entire value added chain from ore extraction right up to the recovery of secondary raw materials.
And, of course, the Plansee Group will be involved. After all, we cover the entire raw materials loop for molybdenum and tungsten. We process ore concentrate to produce metal powders, which form the basis of our products, such as material solutions for flat screens or fuel cells or tool and wear solutions for the mechanical engineering and automotive industries. The Plansee Group collects tools that have reached the end of their service life at its various locations across the world. Well over 50 percent of the tungsten processed in the Plansee Group is recovered from products that have reached the end of their service life.
For more information on the exhibition, visit.