Rods made of molybdenum
Whether for injection molding, in the field of device and machining technology or in the lighting industry: Our rods made of molybdenum and molybdenum alloys excel due to their outstanding material purity and constant high quality.
We place the emphasis on absolute precision during the production of our molybdenum rods. We insist on particularly low tolerances in terms of both diameter and roundness and guarantee rods of exceptional straightness. With our state-of-the-art production equipment and many years of experience in the field of refractory metals, even molybdenum rods of diameters of up to 165 mm are no problem for us.
Because we manufacture our molybdenum rods from especially fine-grained materials, easy forming and machining is guaranteed. Every molybdenum rod we supply is subjected to ultrasound or eddy current testing. Our range includes a number of different surface qualities: lathed, centerless, forged or etched. Tell us your requirements!
Order molybdenum rods online
The following rods made of molybdenum and its alloys can be ordered directly from our online shop. Of course, we are also happy to manufacture customized molybdenum rods. Just contact us!
Rods made of pure molybdenum:
Diameter[mm] | Length[mm] | Quality | Weight[kg] |
---|---|---|---|
2.000 | 500 - 3.000 | ground | 0.032 |
3.00 | 500 - 3.000 | ground | 0.072 |
3.175 | 500 - 3.000 | ground | 0.081 |
4.000 | 500 - 3.000 | ground | 0.128 |
4.750 | 500 - 3.000 | ground | 0.181 |
5.000 | 500 - 3.000 | ground | 0.200 |
6.000 | 500 - 3.000 | ground | 0.288 |
6.350 | 500 - 3.000 | ground | 0.323 |
7.000 | 500 - 3.000 | ground | 0.392 |
7.925 | 500 - 3.000 | ground | 0.503 |
8.000 | 500 - 3.000 | ground | 0.512 |
9.000 | 500 - 3.000 | ground | 0.649 |
9.525 | 500 - 3.000 | forged | 0.726 |
9.525 | 500 - 3.000 | ground | 0.726 |
10.000 | 500 - 3.000 | ground | 0.801 |
12.000 | 500 - 2.000 | ground | 1.153 |
12.000 | 500 - 2.500 | ground | 1.153 |
12.700 | 500 - 2.000 | ground | 1.291 |
12.700 | 500 - 2.000 | forged | 1.291 |
13.000 | 500 - 2.000 | ground | 1.353 |
41.000 | 500 - 2.000 | ground | 1.569 |
15.000 | 500 - 2.000 | forged | 1.802 |
15.000 | 500 - 2.000 | ground | 1.802 |
15.875 | 500 - 2.000 | ground | 2.018 |
16.000 | 500 - 2.000 | forged | 2.05 |
18.000 | 500 - 2.000 | forged | 2.594 |
19.050 | 500 - 1.700 | forged | 2.906 |
19.050 | 500 - 1.700 | forged | 2.906 |
19.050 | 500 - 1.700 | ground | 3.203 |
20.000 | 500 - 1.700 | forged | 3.203 |
22.000 | 500 - 1.700 | ground | 3.875 |
22.225 | 500 - 1.800 | forged | 3.955 |
25.000 | 500 - 2.000 | ground | 5.004 |
25.000 | 500 - 2.000 | forged | 5.004 |
25.400 | 500 - 2.000 | ground | 5.166 |
25.400 | 500 - 2.400 | forged | 5.166 |
30.000 | 500 - 2.000 | ground | 7.206 |
30.000 | 500 - 2.000 | ground | 7.206 |
33.000 | 500 - 2.400 | forged | 8.72 |
35.000 | 500 - 2.000 | forged | 9.809 |
38.100 | 500 - 2.000 | forged | 11.623 |
40.000 | 500 - 2.600 | ground | 12.811 |
45.000 | 500 - 2.200 | forged | 16.576 |
50.800 | 500 - 2.800 | forged | 20.663 |
55.000 | 500 - 2.300 | forged | 24.221 |
60.000 | 500 - 1.800 | forged | 28.825 |
63.500 | 500 - 3.000 | forged | 32.286 |
70.000 | 500 - 1.800 | forged | 39.234 |
80.000 | 500 - 3.000 | forged | 51.245 |
90.000 | 500 - 2.700 | forged | 64.857 |
100.000 | 500 - 2.200 | smooth forged | 80.07 |
120.000 | 500 - 2.000 | smooth forged | 115.301 |
120.000 | 500 - 2.000 | smooth forged | 115.301 |
140.000 | 300 - 500 | smooth forged | 156.937 |
165.000 | 300 - 500 | extruded | 217.991 |
Rods made of titanium-zirconium-molybdenum (TZM):
Diameter[mm] | Length[mm] | Quality | Weight[kg] |
---|---|---|---|
4.750 | 500 - 3.000 | ground | 0.181 |
6.000 | 500 - 3.000 | ground | 0.288 |
6.350 | 500 - 3.000 | ground | 0.323 |
8.000 | 500 - 3.000 | ground | 0.512 |
10.000 | 500 - 3.000 | ground | 0.801 |
12.700 | 500 - 2.000 | forged | 1.291 |
15.875 | 500 - 2.000 | ground | 2.018 |
16.000 | 500 - 1.600 | forged | 2.05 |
18.000 | 500 - 2.000 | forged | 2.594 |
19.050 | 500 - 1.500 | ground | 2.906 |
20.000 | 500 - 2.000 | forged | 3.203 |
22.225 | 500 - 2.000 | forged | 3.955 |
25.000 | 500 - 2.000 | forged | 5.004 |
25.400 | 500 - 1.900 | forged | 5.166 |
26.670 | 500 - 1.800 | forged | 5.695 |
30.000 | 500 - 1.600 | forged | 7.206 |
31.750 | 500 - 1.400 | forged | 8.072 |
33.000 | 500 - 1.400 | forged | 8.72 |
35.000 | 500 - 2.000 | forged | 9.809 |
40.000 | 500 - 3.000 | forged | 12.811 |
45.000 | 500 - 2.000 | forged | 16.214 |
49.500 | 500 - 1.600 | forged | 19.619 |
55.000 | 500 - 1.800 | forged | 24.221 |
63.500 | 500 - 2.800 | forged | 2.05 |
70.000 | 500 - 1.800 | forged | 2.594 |
80.000 | 500 - 2.500 | forged | 2.906 |
90.000 | 500 - 2.300 | forged | 2.906 |
100.000 | 500 - 3.000 | forged | 3.203 |
140.000 | 300 - 500 | forged | 3.203 |
165.000 | 300 - 500 | forged | 3.875 |
A single source for all your needs.
We handle every stage in the manufacture of our molybdenum sheets in-house. From the raw materials through to the finished product. This ensures that you benefit from high-quality at all times.
Order sheets, rods and wire online.

We like to make life easy: a quick and simple ordering process and clearly presented price scales – directly on your screen. Sheets, rods, ribbons and wires as well as products made out of molybdenum, tungsten and tantalum are available for you in configurable dimensions in our online shop!