Online shopMy Plansee
Homepage
Online shopMy Plansee
Materials

Products and applications made from tungsten

Its special properties make tungsten an important material for high-performance applications. Learn more about the application range of tungsten at Plansee. It is used for numerous applications, for example, in the aviation and aerospacemanufacturing technology,  medical technology, and  electronics industries due to its unique property profile.  Our online shop provides an overview of our tungsten semi-finished products. 

  

All information regarding the material tungsten

Applications

What is tungsten used for?

Tungsten is used in a variety of industries, including aviation and aerospace, manufacturing technology, medical technology, and electronics. Its uses in these industries include parts and components that are subject to extreme conditions at high temperatures, such as rocket nozzles, heating elements, and rotating x-ray anodes to create x-ray radiation. Tungsten is used as a heat sink in electronics, for example, because of its high thermal conductivity combined with its low thermal coefficient of expansion. The high thermal and electrical conductivity together with the good wear resistance of tungsten materials make them crucial for use in resistance welding electrodes.

Here's a quick look at tungsten applications and our products that use this material:

Product range

Overview of semifinished products made of tungsten and tungsten alloys

The table provides an overview of our semifinished products made of tungsten. Some of these semifinished products come in a specific thickness or specific range of diameters, while others are available on request.

 

Material Sheets
and
plates
[thickness]
Rods
[diameter]
Wires
[diameter]  
W 0.025 – 20 mm 0.3 – 90 mm 0.025 – 1.50 mm
W-UHP Upon request    
WVM
0.05 – 5 mm 0.3 – 12.99 mm 0.050 – 1.50 mm
WVMW
  13 – 45 mm  
WL05/WL10 Upon request 0.3 – 90 mm 0.010 – 1.50 mm
WC20   Upon request  
WRe05/WRe26   Upon request 0.4 – 1.50 mm
Online shop

Tungsten products in the Plansee online shop

You can order sheets, rods, ribbons, and wires as well as other products in configurable dimensions made of tungsten and tungsten alloys quickly and easily in our online shop.

Take a look at our products in the Plansee online shop

Downloads

Tungsten material brochure and data sheets

Would you like to learn more about tungsten and its alloys? Then please see our material brochure and product data sheets here.

Material brochure: Tungsten
Product data sheet: Tungsten
Product data sheet: Tungsten-rhenium
Other materials

Further refractory metals from Plansee

4295.94
Mo
Molybdenum
73180.95
Ta
Tantalum
W-MMC
Metal Matrix Composites