Straight type


W boat SV10100-50-5027 AC
material W
thickness
(mm)
0,500
width
(mm)
10,0
length
(mm)
100,0
tub length
(mm)
50,0
tub depth
(mm)
2,7
tub capacity
(cc)
0,5
More product informations V tub
 

article  11641719

W boat SV10100-50-5027 AC


list price [EUR]

<10,00 pce 
81,80/pce

≥10,00 pce 
60,30/pce

≥30,00 pce 
47,40/pce


 