Step type


W boat TO16100-30-3429
material W
thickness
(inch)
0.0118
width
(inch)
0.630
length
(inch)
3.937
tub length
(inch)
34.0
tub depth
(inch)
2.9
tub capacity
(cc)
0.6
More product informations oval tub, down step 4.1
 

article  11386682

W boat TO16100-30-3429


list price [USD]

<60,00 pce 
14,80/pce

≥60,00 pce 
10,90/pce

≥150,00 pce 
8,60/pce


 