Step type


W boat TV10100-30-4427
material W
thickness
(mm)
0,300
width
(mm)
10,0
length
(mm)
100,0
tub length
(mm)
44,0
tub depth
(mm)
2,7
tub capacity
(cc)
0,4
More product informations oval tub, upper step 13
 

article  11491742

W boat TV10100-30-4427


list price [EUR]

<70,00 pce 