Straight type


Mo boat SF10100-30-5021
material Mo
thickness
(mm)
0,300
width
(mm)
10,0
length
(mm)
100,0
tub length
(mm)
50,0
tub depth
(mm)
2,1
tub capacity
(cc)
0,5
More product informations flat tub
 

article  11371010

Mo boat SF10100-30-5021


list price [EUR]

<120,00 pce 
5,70/pce

≥120,00 pce 
4,20/pce

≥310,00 pce 
3,30/pce


 