Straight type


material Mo
thickness
(mm)
0,300
width
(mm)
15,0
length
(mm)
100,0
tub length
(mm)
40,0
tub depth
(mm)
3,0
tub capacity
(cc)
1,0
More product informations flat tub
 

article  11371074

Mo boat SF15100-30-4030


list price [EUR]

<90,00 pce 
7,60/pce

≥90,00 pce 
5,60/pce

≥230,00 pce 
4,40/pce


 