Straight type


Mo boat SS17100-20-1528
material Mo
thickness
(inch)
0.0079
width
(inch)
0.669
length
(inch)
3.937
tub length
(inch)
15.0
tub depth
(inch)
2.8
tub capacity
(cc)
0.2
More product informations sphere tub
 

article  11371047

Mo boat SS17100-20-1528


list price [USD]

<100,00 pce 
8,90/pce

≥100,00 pce 
6,60/pce

≥250,00 pce 
5,20/pce


 