Straight type


W boat SF06100-15-4012
material W
thickness
(inch)
0.0059
width
(inch)
0.236
length
(inch)
3.937
tub length
(inch)
40.0
tub depth
(inch)
1.2
tub capacity
(cc)
0.1
More product informations flat tub
 

article  11620420

W boat SF06100-15-4012


list price [USD]

<130,00 pce 
6,40/pce

≥130,00 pce 
4,70/pce

≥340,00 pce 
3,70/pce


 

Service number

Do you have any questions or require any further information?

Service number

GB: + 44 1753 576 959
US: +1 508-918-1300

E-mail address customer service
onlineshop@plansee.com