Straight type


material W
thickness
(inch)
0.0079
width
(inch)
0.591
length
(inch)
3.543
tub length
(inch)
40.0
tub depth
(inch)
2.9
tub capacity
(cc)
1.0
More product informations heat choke
 

article  11456363

W boat SF15090-20-4029 HC


list price [USD]

<60,00 pce 
15,40/pce

≥60,00 pce 
11,40/pce

≥140,00 pce 
8,90/pce


 

Service number

Do you have any questions or require any further information?

Service number

GB: + 44 1753 576 959
US: +1 508-918-1300

E-mail address customer service
onlineshop@plansee.com