Mo tube 12,7 x 1,0 mm
material Mo
outer dia
(mm)
12,700
tol
(mm)
+/-0,1
wall thickness
(mm)
1,000
tol
(mm)
+/-0,1
weight
(kg/m)
0,375
More product informations seamless drawn, tolerance lenght +/- acc. DIN ISO 2768m
 

article  11375018

Mo tube 12,7 x 1,0 mm


list price [EUR]

2.286,27 € (1 kg ) 


Configure product