Rods


material Mo
dia
(mm)
20,000
tol
(mm)
±0,30
length
(mm)
100 - 2200
straightness
(per m)
<1,5 MM
quality/
finish
forged
weight
(kg/m)
3,203
More product informations forged
specification Download
 

article  6622

Mo rod Ø 20,0 mm, forged


list price [EUR]

<1,56 m 
644,60/m

≥1,56 m 
483,45/m

≥3,73 m 
402,88/m

≥9,31 m 
322,30/m


 


Configure product

Service number

Do you have any questions or require any further information?

Service number

GB: + 44 1753 576 959
US: +1 508-918-1300

E-mail address customer service
onlineshop@plansee.com