Rods


material Mo
dia
(mm)
6,350
tol
(mm)
±0,020
length
(mm)
300 - 3000
straightness
(per m)
<1,5 MM
quality/
finish
ground
weight
(kg/m)
0,323
More product informations ground
specification Download
 

article  180932

Mo rod Ø 6,35 mm, ground


list price [EUR]

<12,28 m 
81,45/m

≥12,28 m 
61,09/m

≥29,47 m 
50,91/m

≥73,67 m 
40,73/m


 