Rods


material Mo
dia
(mm)
80,000
tol
(mm)
±1,0
length
(mm)
100 - 3500
straightness
(per m)
<2,5 MM
quality/
finish
forged
weight
(kg/m)
51,245
More product informations forged
specification Download
 

article  132002

Mo rod Ø 80,0 mm, forged


list price [EUR]

<0,11 m 
9.150,81/m

≥0,11 m 
6.863,11/m

≥0,27 m 
5.719,26/m

≥0,66 m 
4.575,41/m


 