Rods


material TaM
dia
(mm)
6,000
tol
(mm)
±0,102
length
(mm)
500 - 2500
straightness
(per m)
<2,5 MM
quality/
finish
pickled
weight
(kg/m)
0,469
More product informations pickled
specification Download
 

article  188161

TaM rod Ø 6,0 mm, pickled


list price [EUR]

<3,00 m 
568,20/m

≥3,00 m 
473,50/m

≥7,00 m 
378,80/m


 