Sheets


material Mo
thickness
(mm)
0,200
tol
(mm)
±0,015
width
(mm)
200,0
tol
(mm)
±0,500
length
(mm)
600,0
tol
(mm)
+5/-0
quality/
finish
bright
weight
(kg/pce)
0,245
More product informations bright, cold rolled, deep drawable
specification Download
 

article  257433

Mo sheet 0,2 x 200 x 600 mm
bright


list price [EUR]

<11,00 pce 
94,81/pce

≥11,00 pce 
71,11/pce

≥26,00 pce 
59,26/pce

≥64,00 pce 
47,41/pce


 

Service number

Do you have any questions or require any further information?

Service number

GB: + 44 1753 576 959
US: +1 508-918-1300

E-mail address customer service
onlineshop@plansee.com