(mm)
0,500
tol
(mm)
±0,020
width
(mm)
600,0
tol
(mm)
±1,600
length
(mm)
2.000,0
tol
(mm)
+5/-0
quality/
finish
bright
weight
(kg/pce)
6,120
More product informations bright, cold rolled; deep drawable
specification Download
 