Sheets


material Mo
thickness
(mm)
0,381
tol
(mm)
±0,020
width
(mm)
609,6
tol
(mm)
±1,600
length
(mm)
10.500,0
tol
(mm)
±10%
quality/
finish
shipment in total coils, pickled
weight
(kg/pce)
24,880
More product informations shipment in total coils, pickled
specification Download
 

article  11039184

Mo sheet 0,381 x 609,6 x min 9450 mm
pickled, shipment in total coils


list price [EUR]

<2,00 pce 
3.387,95/pce

≥2,00 pce 
2.710,36/pce


 

Service number

Do you have any questions or require any further information?

Service number

GB: + 44 1753 576 959
US: +1 508-918-1300

E-mail address customer service